Cooling Question 7

We are having to stop our kiln at frequent intervals because of ring build-ups. When we raise the alumina modulus to ...

Re: Cooling

Ring formation is caused by the formation of liquids in the kiln at a particular position. These penetrate the refrac...

Cooling Question 8

Hot clinker is quenched in water losing useful heat, can you syggest heat recovery without altering process of quench...

Re: Cooling

The white cement clinker must be quenched as it falls from the kiln to freeze the clinker minerals in their high temp...

Cooling Question 9

I want to know about calculation methods of gas and material flow in preheater, pc, kiln, cooler. Further, can you ad...

Re: Cooling

The calculation of gas and material flow in the preheater relies on the principles of stoichoimetry (to assess the co...

Cooling Question 10

I would like information on the formation of “snowmen” in our kiln cooler. Our kiln produces 2000tpd clinker. The kil...

Re: Cooling

Snowman formation is caused by some of the flux in the clinker remaining as a liquid after the clinker falls into the...

Cooling Question 11

What is the effect of cooler dust on flame?