Re: Very Hard coating!!

Is there any difference in fuel or waste derived fuel use in your two kiln?Source of Asulphur may be difference in f...

Re: Very Hard coating!!

It will be better if you may analysed the Na2O,K2O,Cl and SO3 in hotmeal and convert the value in loss free basis a...

Re: Types of rings

Formation of type of ring is based upon the kiln system atmosphere.If sulfur is excess in raw material and fuel than ...

Re: central air pressure

By increasing the air pressure burner tip velocity will be increased and consequently flame momentum will be increase...

Re: Very Hard coating!!

The Molar Ratio can be calculated by the given below formula: Molar Ratio=(SO3/80) / [K2O/94+0.5Na2O/62]-------With...

Re: Kiln balls

Controlling liquid phase level and changing the kiln feed chemistry is better  proactive action or solution to contro...

Re: Very Hard coating!!

The chemical analysis of hotmeal sample revealed that excess sulphur,1418gm per 100 kg of clinke is present in the s...

Re: The lumps in the cement.

  C3A is moisture sensitive mineral.In presence of moisture the C3A of clinker and sulphate of the gypsum from ettr...

Re: European Standards for Cement

You may see at web site www.amazon.com .

Re: Water Spray in front of Finish Mill

It is suggested to do water spray in mill IInd compartment first.If desired cement outlet temperature is not control...