KILN INLET COATING RING

CAN ANYBODY TELL ME HOW CAN I BREAK COATING RING WHICH IS 12-18 METERS INSIDE FROM KILN INLET . KILN LENGTH IS 64 M.

THERE IS A LOT OF HOT MEAL SPILLAGE FROM KILN INLET CONTINOUSLY.

WE HAVE INCREASED RPM OF KILN TO REDUCE THE FILLING DEGREE, REDUCED FEED BY 5% TO REDUCE THE FALL BUT INVAIN.

COAL FIRED IS 75 % OPETCOKE WIH 25 % INDIAN COAL.

CAN I TRY BY FEEDING 50-70MM LIMESTONE AT KILN INLET 10-15 TONS TO BREAK THE RING .

BY REDUCING KILN FILLING SHELL TEMP. ARE MORE THAN 360 DEG.

PL. SUGGEST A SOLUTION

SHALOO

Reply


Know the answer to this question? Join the community and register for a free guest account to post a reply.

kkm
3 posts
TimePosted 08/11/2011 22:10:15
kkm says

Re: KILN INLET COATING RING

dear xxxx,

for breaking kiln inlet ring of this types, only u can increase silica percentage in your raw meal or  put sand into kiln inlet.

have a nice day