HIGH RESIDUE OF PETCOKE IN PRODUCT
DAER ALL
I AM FACING A PROBLEM OF VERY HIGH RESIDUE ON 90 MIC. IN PETCOKE GRINDING VRM IN PRODUCT. IT HAS INCREASED FROM 4% TO 12% OR MORE.
I HAVE CHECKED THE SEPARATOR INTERNALS WHICH IS OUTSIDE THE MILL.
MILL INTERNALS ARE ALSO CHECKED BUT FOUND NO PROBLEM.
ROLLER TENSION IS MAXIMUM [ SPRING LOADED TENSION ON ROLLERS ]
OPERATING PARAMETERS OF FAN SPEED, MILL LOAD, SEPARATOR RPM & LOAD ETC. ARE NORMAL.
TRIED BY CLOSING THE SEPARATOR VAINS BUT NO RESULT.
PLEASE DO ADVISE
ENGR
Know the answer to this question? Join the community and register for a free guest account to post a reply.
153 posts
239 posts
re HIGH RESIDUE OF PETCOKE IN PRODUCT
I have checked , another mill of same dimentions & capacity is running well with less than 4% retn. on 90 mic. Checked sepr . ok . Should I doubt about the grinding effeciency of mill. The operating parameters of mill like mill load, DP, fan load etc. are not reflecting any change. Sepr. static vanes gap reduced to minimum but very high vibn. with high residue etc.
How can I check whether the separator is faulty or the mill?