I am using 100 % petcoke in ILC polysius Kiln [ 7500 tpd].
We have 6% S in petcoke .[ 1.6-1.8% retention on 90 mic.]
LSF in kiln feed 93.6-94%
SM 2
AM 1.2
KF residue 15-17% on 90 mic & 1.7-2% on 212 mic
Kiln filling 12.8-13%
Kiln inlet oxygen 4 to 5%, nil CO
TAD damper full open
Molar ratio 2.6
clinker litre weight 1250-1270
Free lime 0.5 to 0.8%
Flame Momentum 1800-1900 % m/s
Liquid % 28.5-28.9%
Fuel CV 7850-7900
Ash 2-4%
Heat Consumption 720 kcal/kg
We have problems with kiln dusty conditions , ring formation towards kiln inlet ?
How to eleminate such problems permanently?
Any suggestions for change in chemistry or kiln operation parameters and or burner settings etc.