respected members,
Ring formation in Kiln at 37 m and 16 to 20 m area and can any body give me suggetion regarding this issue.
by
BK
If your fuel is pet-coke 37m ring may form due to sulpher condensation
due to dusty kiln
regards
msv
Dear BK
It is a common problem of various plants with number of contributing factors. To find out the best solution for your plant, I need some more details of your kiln system ,burner type and its position wrt kiln, fuel details, kiln operation parameters, kiln feed Chemistry.
For prompt response you can approach me at bilalkkp@gmail.com.
Regards.
Bilal