we are using gas as the main fuel and since they could not supply all the gas for our requirement we are compensating it by using medium grade coal with net cv 5000 kcal and ash content of 35 % and we are using approximately 5 % coal in the precalciner..Kiln side we are using 100 % gas and Precalciner ( PC ) side we are using gas and coal. Whenever there is shortage of gas we are increasing the coal from 5% to 8% approximately. What we are noticing after the increse is Kiln operation disturbs with frequent coating dischage. The cooler gets disturbed and we have to reduce the feed to comeback. The discharged coating looks very hot and molten. Why is it so. Is it because of incresing the coal consumption rate or some other rreeason. There is also the tendency of Bottom stage cyclone jamming. Can somebody give a suggestion