Re: aragonite (CaCO3)

Thank you very much, I reached the information of deltaH formation of aragonite-calcite transformation to be 21j/g...

aragonite (CaCO3)

Hi everyone, In our limestone quarry, there is a small content of aragonite structure of lime. In literature ther...

Re: Preheater fan coating farmation

"Hi everyone, In our plant the top cyclone temperature is around 375 C. The dust recurculating is around 13% of the...

Re: Water injection to the top cyclone

Thank you, I will take my question to there. Our aim for injection of the water to the top cyclone is for reducin...

Re: secondary air temperature

Excellent mr. cantfort:) I have too much to learn in that field :) Let me ask one last question about this topic an...

Water injection to the top cyclone

Hi everyone, In our plant the top cyclone temperature is around 375 C. The dust recurculating is around 13% of the ...

Re: secondary air temperature

You are right Mr. Clark. I'm sure that instead of fluctuation the stabilised low temperature will be better. However...

secondary air temperature

Hi everyone, I've been following the forum for a long time. Thank you very much for your experiences and valuable i...

;