Re: high free lime
There could be a number of reasons of which the most common probably are too coarse raw meal (combinability) or early...
Re: ID FAN AND KILN RPM
With our precalciner kiln we get the best result (clinker reactivity) by operating the kiln close to max speed regar...
Re: Rush in Kiln & heavy coating in KIln inlet
Too high temperature of hotmeal can also cause problems.
Re: FINE CLINKER & REDUCTION IN PRODUCTION
Could be a sulphur problem. Sulphur affects the melt viscosity and tends to make the clinker more dusty. What is the...
Re: snowman on burner pipe
Ted Of course you are right about dust - I just wanted to mention the other possibility. I chose Belite as a mod...
Re: snowman on burner pipe
It may not be dust. If the burner protrudes into the kiln, the reason may very well be that sticky materials (e.g. s...