I am working out the percentage by-pass required for a large precalciner-preheater kiln for the production of low alk...
There is no absolute relationship between chloride content and alkali volatility. This depends on the other anoins pr...
I would like to know how to get rid of the rings that occurs around upper transition zone without mechanically breaki...
There are various options, but if you cannot avoid the problem by better control of the kiln feed chemistry or burnin...
What are the relationships between clinker hard burning and grindability of clinker. Is hard burned clinker hard to g...
When clinker is hard burnt the amount of liquid phase increases and the clinker becomes very dense and fused together...
We are getting build-ups of material on the discharge flaps, Can you advise how to stop the same?
The only thing can suggest is that you carefully adjust the counter-weights on the cyclone discharge flaps so that th...
We carry out refractory work with screw jacks, maximum 10m lining at a time (ie 5m maximum simultaneously at two diff...
I would recommend using the glueing method rather than screw jacks and then you can replace as long a section as you ...
;