Have you calculated the velocity inside the TAD?It should be Greater than 25 m/sec.If the carrying velocity is less ...
Dear XXXX, can I have your calculation methodology?Based on that i can help you.
Dear prisoner, Kiln ID will be same throughout the length but OD will vary due to thickness of the kiln vary from 3...
Good Excel format for the begineers..
For Conveying the cement in any pneumatic conveying: During winter : Maintain the temperature of 70-90 deg C. Du...
pl reply me that where the material is there?either cooler side or calciner side? Design of TAD? Any settling cham...
Dear el, I hope i'm here to solve your query? Your calculation should be of two basis: upto clinkerisation,crushi...
Dear Mr.Rao, Since the pet coke is small size balls,its table retention time has to be increased,my only suggestion...
Dear Mr.Wahid, pl send me your Mill complete details like Any recent changes to the Mill? Any changes in the clin...
Dear Prisoner, Ted is correctly replied that the formation of C2S begins @ the temperature range of 900-1050 deg C,...
;