If one mill is enough and you do not need the second one then go on and good luck. Start study the process, sulfati...
Hi Gulam You have to aware that R90u should be below 5% with petcoke. And with coal depending on volatility coul...
Please do not go to much into chemistry of the process and mineralogy of clinker. It is too early. Are you sure your ...
45 minutes is very low... Even 95 is strange for me. What standard do you have???? Definitely not EN-197 1. Check wha...
Hi I do not think that retention time is critical parameter for grinding optimization. Focus on the ball charge dis...
elwathig: what the optimum position for nozzle pipe tip inside the kiln? At the kiln outlet. No need to g...
I mean the build ups are caused also by bad state of the walls. So we need to close all pors with some good paint, or...
In our case it is driven also by moisture penetration through the walls (bad luck)
The calciner itself cannot make reducing atmosphere. It is a matter of fuel physical state, orifice cross-section, a...
I think the burner was not set to the kiln axis. Last time we did correct adjustement and our CO decreased for 30-40%...
;