Hello Dastgir, The only time you would be able to take a representative slice of a stockpile end-cone would be at r...
vinayak: It can be improved by increasing the number of layers by increasing the stacker speed. Yes, ...
Hi Tam, We had this same problem at my plant several years ago. In the end, we installed a PGNA cross-belt analy...
Hi Davo, The ASR has to do with soluble alkalis, so that even with respect to clinker, only the soluble alkali port...
Hello Raj, Coincidentially we had the same experience in our 5000tpd, dual string preheater, precalciner kiln last ...
Hello Raj, The Magotteaux test is a fairly simple but very sensitive test for the presence of Fe2+ in clinker, alt...
While reduced iron can lead to the phenomenon of brown or yellow centres in clinker nodules as described above, I ha...
Hello Tam. I have seen values of >2% clay in concrete quoted as causing problems. I believe there is a titratio...
Hello Gulam, It really depends on how long the clinker has been exposed to moisture and whether or not it has also ...
Hi, We did this exercise in 2004 when we converted our old 125t/h, single string cyclone preheater kiln into a 36t...
;