Unfortunately these problems are regularly reported on kilns burning petroleum coke. The problem is caused by the sul...
What would be the recommended ball charge and combination to produce masonry cement at 6000 cm 2 /g. the component pe...
I am not surprised that you could not find what you were looking for by research. You will have to find the optimum b...
We have a plant of short kiln with two stations 52m length and 4.8m dia since some months we are facing problem of re...
These temperatures are serious and will damage the kiln. You need to change the kiln chemistry to adjust the flux con...
We have problem of hard clinker used in cement grinding. This clinker is produced by using 100 per cent pet coke in f...
I have looked at the photomicrographs and read your analysis with interest. In order to properly answer your question...
We have faced the serious coating formation at 12 to 26 meter of Kiln and plant have to be forced stopped for coating...
I have studied the data you have submitted. We receive regular reports of heavy coating and ball formation associated...
I am a consultant to the petroleum coke industry. There is a lot of talk that high sulphur pet coke (7-8 per cent) ...
;