Avatar

AN - Kuwait

Registered User

Re: Mill Draught

Roughly the outlet draught is 30 times ID in mm .And you can calculate by taking the empty volume of mill,residence t...

Re: Hurrivanes

Dear Raj, I do not have the old ICR.How can I get it.   

Re: kiln RPM increasing

Gear box ratio is required and the other parmeters like Volumetric load,power max.capacity.And also if you change the...

Re: Use artificial gypsum for cement

Characteristics will be same only cost calculations you have to do.If it is commerecially OK that you can save some m...

Re: JPF Fan impiller coating

Hi, There are two solutions 1) .You can introduce fine sand from the downcomer duct at regular intervals.2) Install...

Hurrivanes

Dear Clark ,  What is the Hurriclone/Hurrivane technology? We have 5th stage PH system LP Cyclones.Can we try Hurr...

Re: How much velocity to be maintaine across the ball mill

1.5m/sec.for closed circuit and 1 m/s for open circuit.

Re: JPF Fan impiller coating

Take the sample of the coating and check it for Fe may be the raw mix composition is changed from previous to now.

Re: % of grinding media in ball mills for both chambers

You can get FLS COMMUNITION MANUAL which will give you the tables regarding the calculations.And also how to estimat...

Re: Length of flame

The length of the flame in general will be 2.5 - 3 times of kiln Diameter.

;