Dear all,

My kiln capacity is 4500 TPD, but we are operating it at 5400 TPD. My problem is clinker litre weights are higher side i.e. > 1270 g. But I want to maintaine around 1200 g. Can any body suggest me is there any way to reduce the clinker litre weights by changing the raw mix design, if so request you to share the information.

In view of to reduce clinker litre weights I have tried by reducing kiln coal consumption in tern burning zone temperature. But when ever clinker litre weights are falling down <1250g immediately burning zone is becoming little bit dusty and blocking the secondary air entry into kiln which resulting reduction atmospere in kiln and causing to reduce the production. So I want to concentrate on raw mix design.

Regards,