Avatar

vinayak

Registered User

Re: Heat Balance

Hi As you know, it is very difficult to explain the heat balance in this forum and it needs atleast 3 hours to dis...

Re: Coating formation in Kiln Inlet

Hi Coating at kiln inlet ia mainly due to the volatiles like Chlorides, alkalies ( Na2O and K2O) and SO3. To minimi...

Re: Heat Balance

Hi You can refer the training coarse material given by FLS or Wholcim.Onceyou made the format ready in excel sheet ...

Re: Kiln hood

Hi Normal life of hood arches is about 2 to 3 years. I don't expect a design problem.It is very difficult to come t...

Re: Clinker High Liter Weight and High Free Lime

Hi If that is the case the following may be tried 1. By increasing the rawmeal fineness 2. By increasing the calc...

Re: Clinker High Liter Weight and High Free Lime

hi If it does not happen we can diagonise( just kidding). When you reduce the liter weight you would have reduced ...

Re: central air pressure

Hi friends I hope that both of you are correct. But only the conditions are different. For the same flow, as in t...

Re: kiln manhole location

Hi Apart from the kiln load factors, normally near the second tyre a mnahole provided to remove the used bricks and...

Re: Thermal load

Hi You may multiply the fuel feed by CV For ex Kiln fuel feed rate  = 6000 kgs/hr C.V                     = 6500 ...

;