Bhaskar Agate
Posts: 84
Strapline: Registered User
Location: Pune (Maharashtra) INDIA
Occupation: Trainer-Guest/visiting faculty
Posts
Re: The residual moisture content of pulverized coal/petcoke
Dear Firat, Around 1-2% moisture should be adequate for proper ignition Best Wishes Bhaskar Agate
Re: Clinker litreweight vs Free lime
Normal 0 false false false MicrosoftInternetExplo...
Re: high free lime and liter weight
Your clinker LSF appears to be very high.SM you have not mentioned.It would be desirable to bring down LSF gradually...
Re: clinker temperature
You need to find out the competent consultants/agency in your area who can perform heat and mass balance for your ki...
Re: clinker temperature
A thorough study (Heat,mass & air balance) should help you to identify the actual problem in cooler & kiln system in...
Re: high free lime and liter weight
Adjustment of LSF 98-99 and SM 2.4-2.6 with AM 1.6 may please be attempted for raw meal and accordingly individual c...
Re: Clinker litreweight vs Free lime
Dear All, An article has been published in ICR Aug.10 th issue page no.70 on the subject title "Quality Control of...
Re: material build up
It has been experienced that water spray in cooler invariably results into build ups and requires periodical cleanin...
Re: Retainer Ring inside Kiln
Retainer ring provide support at the end of brick lining thereby restricting the sliding motion of bricks downward w...
Re: Cement Standard
When the cement was invented it is said that it is resembling Portland stone/rock. Ordinary word might have been coi...