viswam
Posts: 15
Strapline: Registered User
Location:
Occupation:
Posts
re Re: Kiln Inlet Coating
we are using 100 % petcoke as a fuel, we face every start up 35 - 40 m between ring Avoid kiln Inlet spillag...
re ring in kiln
Hello Mr Raj Sahu, last month 3 times we have stopped the kiln for breaking sinter ring even though we have...
re Raw mix.Design
Mr Ted For trial purpose only we have done it but it is not giving good result thank you
re Raw mix.Design
Hello Mr. Ted, Unfortunately if we missed to correct the pile, shall we feed the corrective material t...
re Ring formation inside the Kiln
If your fuel is pet-coke 37m ring may form due to sulpher condensation due to dusty kiln regards msv
re Impact of ALKALY, SULPHURE and CHLORINE in Kiln operation and clinker quality ?
Thanks.
re Impact of ALKALY, SULPHURE and CHLORINE in Kiln operation and clinker quality ?
Thank you sir I need one more suggestion from you. we are using 100 % pet coke as fuel we have a PID cont...
re Impact of ALKALY, SULPHURE and CHLORINE in Kiln operation and clinker quality ?
Sir, Our's is 5 stage pre-heater ILC kiln we are using 100 pet coke as fuel smoke chamber coating is form...
re Copper (Cu) impact on clinker or cement quality?
Is there any limit for Copper slag usage thanks
100 % pet coke as a fuel
Sir we are faceing burning problem of during long stoppage of raw mill regards msv